- June 30, 2001, ... strength of the PSA. DOP causes a drastic drop in SAFT and shear. The failure mode in the 180∞ peel test switches from a clean peel off the steel to a cohesive failure within the adhesive layer. Testing ...
- Cast Film Dies and Auxiliary Equipment
- (Magazine)
- February 28, 2001, ... temperature and be heated appropriately to the melt temperature of the polymer they are conveying. To size a melt pipe correctly requires balancing pressure drop and residence time. A longer transfer pipe ...
- Products
- (Magazine)
- December 31, 2000, ... and computer-controlled programmer provide a roll length accuracy of 0.1 in. (2.5 mm) at speeds to 1,000 fpm (305 mpm). Options include automatic splice detection and defective roll dropout, video web ...
- Curtain Coating Technology Can Mean Big Benefits
- (Magazine)
- February 29, 2000, ... perpendicular relative to the gravity vector. However, it may be advantageous or necessary to drop the curtain onto a web with an uphill or downhill orientation, for example, if the coating machine has ...
- Coextrusion: making the equipment fit the need
- (Magazine)
- June 30, 1996, ... the material becomes more viscous, and output drops dramatically. According to Wheeler, Windmoeller & Hoelscher equipment can convert the revolutionary raw material without change. In fact, says Wheeler, ...